Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Adhesion | 23.0 °C | 93 N Show Supplier Material materials with Adhesion of 93 N | min., Hot U Test |
Lineare Dichte | 23.0 °C | 3.9E-3 - 4.5E-3 g/cm Show Supplier Material materials with Lineare Dichte of 3.9E-3 - 4.5E-3 g/cm |
Abmessung
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Nominal breaking force | 23.0 °C | 240 N Show Supplier Material materials with Nominal breaking force of 240 N | Tensile Member: E Glass |
Technological properties
Property | ||
---|---|---|
Color | Black | |
Cord Construction | 330.1/0 | |
Other | Manufacturing Location: Canada | |
Processing history | Latex Type: Chloroprene, Dip Pick-Up: 19 to 28% | |
Twist per Meter | 106 - 134 TPM | Direction: S & Z |