Allgemein
Abmessung
Property | Value | Comment |
---|---|---|
Bobbin Inner Diameter | 60 mm Show Supplier Material materials with Bobbin Inner Diameter of 60 mm | |
Bobbin Length | 356 mm Show Supplier Material materials with Bobbin Length of 356 mm | |
Durchmesser | 0.7 - 1.3 mm Show Supplier Material materials with Durchmesser of 0.7 - 1.3 mm | Apparent Diameter |
Flange Diameter | 190.5 mm Show Supplier Material materials with Flange Diameter of 190.5 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Nominal breaking force | 23.0 °C | 670 N Show Supplier Material materials with Nominal breaking force of 670 N | Tensile Member: E Glass |
Technological properties
Property | ||
---|---|---|
Color | Brown | |
Cord Construction | 330.1/3 | |
Other | Manufacturing Location: Canada | |
Processing history | Latex Type: SBR, Dip Pick-Up: 17 to 23% | |
Twist per Meter | 70 - 90 TPM | Direction: S & Z |