Property | Value | Comment |
---|---|---|
Bobbin Inner Diameter | 57 - 63 mm Show Supplier Material materials with Bobbin Inner Diameter of 57 - 63 mm | tapered |
Bobbin Length | 341 mm Show Supplier Material materials with Bobbin Length of 341 mm | |
Durchmesser | 0.9 - 1.5 mm Show Supplier Material materials with Durchmesser of 0.9 - 1.5 mm | Apparent Diameter |
Flange Diameter | 279.5 mm Show Supplier Material materials with Flange Diameter of 279.5 mm |
Mechanisch
Technological properties
Property | ||
---|---|---|
Color | Black | |
Cord Construction | 330.1/4 | |
Other | Manufacturing Location: Canada | |
Processing history | Latex Type: Chloroprene, Dip Pick-Up: 19 to 28% | |
Twist per Meter | 69 - 89 TPM | Direction: S & Z |