Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Adhesion | 23.0 °C | 125 N Show Supplier Material materials with Adhesion of 125 N | min., Hot U Test |
Lineare Dichte | 23.0 °C | 0.01 - 0.02 g/cm Show Supplier Material materials with Lineare Dichte of 0.01 - 0.02 g/cm |
Abmessung
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Nominal breaking force | 23.0 °C | 890 N Show Supplier Material materials with Nominal breaking force of 890 N | Tensile Member: E Glass |
Technological properties
Property | ||
---|---|---|
Color | Brown | |
Cord Construction | 330.1/4 | |
Other | Manufacturing Location: Canada | |
Processing history | Latex Type: Chloroprene, Dip Pick-Up: 9 to 13.5% | |
Twist per Meter | 70 - 90 TPM | Direction: S & Z |