Allgemein
Property | Temperature | Value |
---|---|---|
Lineare Dichte | 23.0 °C | 0.1 - 0.11 g/cm Show Supplier Material materials with Lineare Dichte of 0.1 - 0.11 g/cm |
Abmessung
Property | Value | Comment |
---|---|---|
Bobbin Inner Diameter | 57 - 63 mm Show Supplier Material materials with Bobbin Inner Diameter of 57 - 63 mm | tapered |
Bobbin Length | 341 mm Show Supplier Material materials with Bobbin Length of 341 mm | |
Flange Diameter | 279.5 mm Show Supplier Material materials with Flange Diameter of 279.5 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Nominal breaking force | 23.0 °C | 4000 N Show Supplier Material materials with Nominal breaking force of 4000 N | Tensile Member: E Glass |
Technological properties
Property | ||
---|---|---|
Color | Black | |
Cord Construction | 330.3/8 | |
Other | Manufacturing Location: Canada | |
Processing history | Latex Type: Chloroprene, Dip Pick-Up: 19 to 28% | |
Twist per Meter | 32 - 44 TPM | Direction: S & Z |