Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materialien
Categories
Sie sind nicht angemeldet
Categories
Metalllieferanten finden
List Your Company
Case Studies
Tools
Über uns
Chopped Strand G99-003007
NBR latex impregnated carbon fibre chopped strand (Elastomer Polymer Matrix Composite)
Diese Materialdaten wurden von NGF Glass zur Verfügung gestellt
All categories
Allgemein
Property | Temperature | Value |
---|---|---|
Lineare Dichte | 23.0 °C | 0.01 g/cm Show Supplier Material materials with Lineare Dichte of 0.01 g/cm |
Abmessung
Property | Value | Comment |
---|---|---|
Länge | 2 - 6 mm Show Supplier Material materials with Länge of 2 - 6 mm | Chopped Strand |
Technological properties
Property | ||
---|---|---|
Color | Black | |
Other | Manufacturing Location: Canada | |
Processing history | Latex Type: NBR, Dip Pick-Up: 20 to 30% |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
UNTERNEHMEN
KONTAKTIEREN SIE UNS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.