Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Adhesion | 23.0 °C | 196 N Show Supplier Material materials with Adhesion of 196 N | min., T Test |
Lineare Dichte | 23.0 °C | 0.01 g/cm Show Supplier Material materials with Lineare Dichte of 0.01 g/cm | |
Loss on Ignition | 23.0 °C | 16 - 21 % Show Supplier Material materials with Loss on Ignition of 16 - 21 % |
Abmessung
Property | Value | Comment |
---|---|---|
Bobbin Inner Diameter | 57 - 64 mm Show Supplier Material materials with Bobbin Inner Diameter of 57 - 64 mm | tapered |
Bobbin Length | 305 mm Show Supplier Material materials with Bobbin Length of 305 mm | |
Durchmesser | 0.98 - 1.12 mm Show Supplier Material materials with Durchmesser of 0.98 - 1.12 mm | Apparent Diameter |
Flange Diameter | 152.5 mm Show Supplier Material materials with Flange Diameter of 152.5 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 2.1 - 3.5 % Show Supplier Material materials with Dehnung of 2.1 - 3.5 % | |
Nominal breaking force | 23.0 °C | 589 N Show Supplier Material materials with Nominal breaking force of 589 N | Tensile Member: E Glass |
Technological properties
Property | ||
---|---|---|
Color | Black | |
Cord Construction | 110.1/10 | |
Other | Manufacturing Location: UK / Poland | |
Processing history | Latex Type: Chloroprene | |
Twist per Meter | 106 - 130 TPM | Direction: S & Z |