Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Adhesion | 23.0 °C | 90 N Show Supplier Material materials with Adhesion of 90 N | min., T Test |
Lineare Dichte | 23.0 °C | 2.5E-3 - 2.9E-3 g/cm Show Supplier Material materials with Lineare Dichte of 2.5E-3 - 2.9E-3 g/cm | |
Loss on Ignition | 23.0 °C | 16 - 21 % Show Supplier Material materials with Loss on Ignition of 16 - 21 % |
Abmessung
Property | Value | Comment |
---|---|---|
Bobbin Inner Diameter | 60 mm Show Supplier Material materials with Bobbin Inner Diameter of 60 mm | |
Bobbin Length | 360 mm Show Supplier Material materials with Bobbin Length of 360 mm | |
Durchmesser | 0.4 - 0.5 mm Show Supplier Material materials with Durchmesser of 0.4 - 0.5 mm | Apparent Diameter |
Flange Diameter | 139 mm Show Supplier Material materials with Flange Diameter of 139 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 1.4 - 3.6 % Show Supplier Material materials with Dehnung of 1.4 - 3.6 % | |
Nominal breaking force | 23.0 °C | 120 N Show Supplier Material materials with Nominal breaking force of 120 N | Tensile Member: E Glass |
Technological properties
Property | ||
---|---|---|
Color | Black | |
Cord Construction | 110.1/2 | |
Other | Manufacturing Location: UK / Poland | |
Processing history | Latex Type: Chloroprene | |
Twist per Meter | 124 - 160 TPM | Direction: S & Z |