Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Adhesion | 23.0 °C | 59 N Show Supplier Material materials with Adhesion of 59 N | min., T Test |
Lineare Dichte | 23.0 °C | 1.2E-3 - 1.5E-3 g/cm Show Supplier Material materials with Lineare Dichte of 1.2E-3 - 1.5E-3 g/cm | |
Loss on Ignition | 23.0 °C | 16 - 22 % Show Supplier Material materials with Loss on Ignition of 16 - 22 % |
Abmessung
Property | Value | Comment |
---|---|---|
Bobbin Inner Diameter | 57 - 64 mm Show Supplier Material materials with Bobbin Inner Diameter of 57 - 64 mm | tapered |
Bobbin Length | 305 mm Show Supplier Material materials with Bobbin Length of 305 mm | |
Durchmesser | 0.16 - 0.3 mm Show Supplier Material materials with Durchmesser of 0.16 - 0.3 mm | Apparent Diameter |
Flange Diameter | 152.5 mm Show Supplier Material materials with Flange Diameter of 152.5 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 1.8 - 3.4 % Show Supplier Material materials with Dehnung of 1.8 - 3.4 % | |
Nominal breaking force | 23.0 °C | 59 N Show Supplier Material materials with Nominal breaking force of 59 N | Tensile Member: E Glass |
Technological properties
Property | ||
---|---|---|
Color | Black | |
Cord Construction | 110.1/0 | |
Other | Manufacturing Location: UK / Poland | |
Processing history | Latex Type: Chloroprene | |
Twist per Meter | 154 - 177 TPM | Direction: S & Z |