Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Adhesion | 23.0 °C | 120 N Show Supplier Material materials with Adhesion of 120 N | min., T Test |
Lineare Dichte | 23.0 °C | 0.02 g/cm Show Supplier Material materials with Lineare Dichte of 0.02 g/cm | |
Loss on Ignition | 23.0 °C | 17 - 23 % Show Supplier Material materials with Loss on Ignition of 17 - 23 % |
Abmessung
Property | Value | Comment |
---|---|---|
Bobbin Inner Diameter | 57 - 63 mm Show Supplier Material materials with Bobbin Inner Diameter of 57 - 63 mm | tapered |
Bobbin Length | 341 mm Show Supplier Material materials with Bobbin Length of 341 mm | |
Durchmesser | 1.12 - 1.28 mm Show Supplier Material materials with Durchmesser of 1.12 - 1.28 mm | Apparent Diameter |
Flange Diameter | 279.5 mm Show Supplier Material materials with Flange Diameter of 279.5 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 2.4 - 3.8 % Show Supplier Material materials with Dehnung of 2.4 - 3.8 % | |
Nominal breaking force | 23.0 °C | 883 N Show Supplier Material materials with Nominal breaking force of 883 N | Tensile Member: E Glass |
Technological properties
Property | ||
---|---|---|
Color | Black | |
Cord Construction | 110.1/13 | |
Other | Manufacturing Location: UK / Poland | |
Processing history | Latex Type: Chloroprene | |
Twist per Meter | 72 - 88 TPM | Direction: S & Z |