Property | Temperature | Value |
---|---|---|
Lineare Dichte | 23.0 °C | 3.5E-3 - 4.5E-3 g/cm Show Supplier Material materials with Lineare Dichte of 3.5E-3 - 4.5E-3 g/cm |
Loss on Ignition | 23.0 °C | 19.5 - 25.5 % Show Supplier Material materials with Loss on Ignition of 19.5 - 25.5 % |
Abmessung
Property | Value | Comment |
---|---|---|
Bobbin Inner Diameter | 57 - 63 mm Show Supplier Material materials with Bobbin Inner Diameter of 57 - 63 mm | tapered |
Bobbin Length | 341 mm Show Supplier Material materials with Bobbin Length of 341 mm | |
Durchmesser | 0.4 - 0.6 mm Show Supplier Material materials with Durchmesser of 0.4 - 0.6 mm | Apparent Diameter |
Flange Diameter | 279.5 mm Show Supplier Material materials with Flange Diameter of 279.5 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Nominal breaking force | 23.0 °C | 177 N Show Supplier Material materials with Nominal breaking force of 177 N | Tensile Member: E Glass |
Technological properties
Property | ||
---|---|---|
Color | Black Overcoat | |
Cord Construction | 34.3/3 | |
Other | Manufacturing Location: UK | |
Processing history | Latex Type: HNBR | |
Twist per Meter | 108 - 132 TPM | Direction: S & Z |