Allgemein
Property | Temperature | Value |
---|---|---|
Lineare Dichte | 23.0 °C | 0 - 0.02 g/cm Show Supplier Material materials with Lineare Dichte of 0 - 0.02 g/cm |
Loss on Ignition | 23.0 °C | 0.3 - 0.6 % Show Supplier Material materials with Loss on Ignition of 0.3 - 0.6 % |
Abmessung
Property | Value |
---|---|
Bobbin Inner Diameter | 76 mm Show Supplier Material materials with Bobbin Inner Diameter of 76 mm |
Mechanisch
Property | Value |
---|---|
Nominal breaking force | Tensile Member: U Glass |
Technological properties
Property | ||
---|---|---|
Color | White | |
Cord Construction | Roving | |
Other | Manufacturing Location: Japan | |
Processing history | Latex Type: Plastic Size | |
Twist per Meter | No Twist |