Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.83 g/cm³ Show Supplier Material materials with Dichte of 7.83 g/cm³ |
Abmessung
Property | Value |
---|---|
Außendurchmesser | 450 - 910 mm Show Supplier Material materials with Außendurchmesser of 450 - 910 mm |
Breite | 1350 - 2540 mm Show Supplier Material materials with Breite of 1350 - 2540 mm |
Dicke | 150 - 230 mm Show Supplier Material materials with Dicke of 150 - 230 mm |
Innendurchmesser | 400 - 730 mm Show Supplier Material materials with Innendurchmesser of 400 - 730 mm |
Länge | 1750 - 3370 mm Show Supplier Material materials with Länge of 1750 - 3370 mm |
Chemical properties
Property | Value |
---|---|
Arsen | 0 - 0.08 % Show Supplier Material materials with Arsen of 0 - 0.08 % |
Chrom | 0 - 0.25 % Show Supplier Material materials with Chrom of 0 - 0.25 % |
Eisen | Balance |
Kohlenstoff | 0.42 - 0.5 % Show Supplier Material materials with Kohlenstoff of 0.42 - 0.5 % |
Kupfer | 0 - 0.25 % Show Supplier Material materials with Kupfer of 0 - 0.25 % |
Mangan | 0.5 - 0.8 % Show Supplier Material materials with Mangan of 0.5 - 0.8 % |
Nickel | 0 - 0.25 % Show Supplier Material materials with Nickel of 0 - 0.25 % |
Phosphor | 0 - 0.04 % Show Supplier Material materials with Phosphor of 0 - 0.04 % |
Schwefel | 0 - 0.04 % Show Supplier Material materials with Schwefel of 0 - 0.04 % |
Silizium | 0.17 - 0.37 % Show Supplier Material materials with Silizium of 0.17 - 0.37 % |
Technological properties
Property | ||
---|---|---|
Application areas | Steel forgings are applied for manufacture of the details of machinery and spare parts for metallurgical, mining and machine-building equipment. | |
Processing methods | Manufactured by open die forging |