Allgemein
Property | Value | Testing Standard | Comment |
---|---|---|---|
Bonding strength | 907.2 Kg Show Supplier Material materials with Bonding strength of 907.2 Kg | ASTM D229 | Condition A |
Dichte | 1.34 g/cm³ Show Supplier Material materials with Dichte of 1.34 g/cm³ | ASTM D792 | |
Moisture absorption | 2.3 % Show Supplier Material materials with Moisture absorption of 2.3 % | ASTM D570 | Condition A |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Biegefestigkeit | 127.6 MPa Show Supplier Material materials with Biegefestigkeit of 127.6 MPa | ASTM D790 | Condition A, Transverse |
168.9 MPa Show Supplier Material materials with Biegefestigkeit of 168.9 MPa | ASTM D790 | Condition A | |
Biegemodul | 9 GPa Show Supplier Material materials with Biegemodul of 9 GPa | ASTM D790 | Condition A, Transverse |
11.7 GPa Show Supplier Material materials with Biegemodul of 11.7 GPa | ASTM D790 | Condition A | |
Druckfestigkeit | 262 MPa Show Supplier Material materials with Druckfestigkeit of 262 MPa | ASTM D695 | Condition A | Flatwise |
Härte, Rockwell M | 100 [-] Show Supplier Material materials with Härte, Rockwell M of 100 [-] | ASTM D785 | |
Impact strength, Izod unnotched, ASTM | 72 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 72 J/m | ASTM D256 | Condition E-48/50, Transverse |
91 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 91 J/m | ASTM D256 | Condition E-48/50 | |
Scherfestigkeit | 93.1 MPa Show Supplier Material materials with Scherfestigkeit of 93.1 MPa | ASTM D732 | Condition A, Transverse |
Zugfestigkeit | 96.5 MPa Show Supplier Material materials with Zugfestigkeit of 96.5 MPa | ASTM D638 | Condition A |
Thermisch
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 1.8e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.8e-05 1/K | IPC-TM 650-2.4.24 | |||
1.9e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.9e-05 1/K | IPC-TM 650-2.4.24 | Transverse | |||
Relative temperature index, electrical | 115 °C Show Supplier Material materials with Relative temperature index, electrical of 115 °C | UL Bulletin 746b¹ | |||
Relative temperature index, mechanical strength | 125 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 125 °C | UL Bulletin 746b¹ | |||
Arc resistance | 15 seconds, ASTM D495, Condition A | ||||
Entflammbarkeit | UL Bulletin 94, Class HB, Condition A |
Elektrisch
Property | Value | Frequency | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 5.8 [-] Show Supplier Material materials with Dielektrizitätskonstante of 5.8 [-] | 1MHz | ASTM D150 | Condition D-24/23 |
Durchschlagfestigkeit | 17.72 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 17.72 kV/mm | ASTM D149 | Condition D-48/50 | |
22.64 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 22.64 kV/mm | ASTM D149 | Condition A | ||
Durchschlagspannung | 2 kV Show Supplier Material materials with Durchschlagspannung of 2 kV | ASTM D149 | Condition D48/50 | |
45 kV Show Supplier Material materials with Durchschlagspannung of 45 kV | ASTM D149 | Condition A | ||
Kriechstromfestigkeit | 170 V Show Supplier Material materials with Kriechstromfestigkeit of 170 V | ASTM D3638 | ||
Verlustfaktor | 0.07 [-] Show Supplier Material materials with Verlustfaktor of 0.07 [-] | 1MHz | ASTM D150 | Condition D-24/23 |
Technological properties
Property | ||
---|---|---|
Fillers | Cotton Fabric | |
Other | 1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |