Polyamide 66 (PA66)
Zytel® 70G25HSL NC010Polyamide 6T (PA6T)
Zytel® HTN51G35HSL NC010Polyamide 66 (PA66)
Zytel® 70G25HSLR NC010Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00Wrought Copper High Copper Alloy
ASTM B194 Grade C17200 TD04Austenitischer rostfreier Stahl
Sandvik 253 MAGeliefert von:
Alleima (formerly Sandvik Materials Technology)Wrought Copper High Copper Alloy
EN 1652 Grade C17200 TF00Polyamide 6T (PA6T)
Zytel® HTN51G35EF BK083Polyphenylene Sulfide (PPS)
RADITECK P RCM651K 1700 NTGeliefert von:
RadiciGroup High Performance Polymers