Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 0.83 - 0.89 g/cm³ Show Supplier Material materials with Dichte of 0.83 - 0.89 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dehnung | 1100.6 % Show Supplier Material materials with Dehnung of 1100.6 % | ASTM D412 | min. | 500 mm/min |
Härte, Shore A | 7 - 13 [-] Show Supplier Material materials with Härte, Shore A of 7 - 13 [-] | ASTM D2240 | |
Modul bei 100 % Dehnung | 0.00015 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.00015 GPa | ASTM D412 | 500 mm/min |
Modul bei 300 % Dehnung | 0.00023 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.00023 GPa | ASTM D412 | 500 mm/min |
Reißfestigkeit | 8.8 kN/m Show Supplier Material materials with Reißfestigkeit of 8.8 kN/m | ASTM D624 Die C | 500 mm/min |
Zugfestigkeit | 2.7 MPa Show Supplier Material materials with Zugfestigkeit of 2.7 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 11.2 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 11.2 g/10min | ASTM D1238 | 190°C/1.2kg |
Schrumpfung | 2.2 - 2.8 % Show Supplier Material materials with Schrumpfung of 2.2 - 2.8 % | ASTM D955 | Transverse |
2.3 - 2.9 % Show Supplier Material materials with Schrumpfung of 2.3 - 2.9 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Shoes insole, medical appliances, fishing lure, sports equipment, toys | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | Transparent | |
Other | Overmolding capabilities: PP |