Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 0.84 - 0.9 g/cm³ Show Supplier Material materials with Dichte of 0.84 - 0.9 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dehnung | 652.3 % Show Supplier Material materials with Dehnung of 652.3 % | ASTM D412 | 500 mm/min |
Härte, Shore A | 27 - 33 [-] Show Supplier Material materials with Härte, Shore A of 27 - 33 [-] | ASTM D2240 | |
Modul bei 100 % Dehnung | 0.00052 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.00052 GPa | ASTM D412 | 500 mm/min |
Modul bei 300 % Dehnung | 0.00102 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.00102 GPa | ASTM D412 | 500 mm/min |
Reißfestigkeit | 11.8 kN/m Show Supplier Material materials with Reißfestigkeit of 11.8 kN/m | ASTM D624 Die C | 500 mm/min |
Zugfestigkeit | 3.4 MPa Show Supplier Material materials with Zugfestigkeit of 3.4 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 42.8 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 42.8 g/10min | ASTM D1238 | 190°C/1.2kg |
Schrumpfung | 1.3 - 1.9 % Show Supplier Material materials with Schrumpfung of 1.3 - 1.9 % | ASTM D955 | Transverse |
1.5 - 2.1 % Show Supplier Material materials with Schrumpfung of 1.5 - 2.1 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Pen grip, toothbrush, bike grip, teether, nursing appliances | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | Transparent | |
Other | Overmolding capabilities: PP |