Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 1.06 - 1.12 g/cm³ Show Supplier Material materials with Dichte of 1.06 - 1.12 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 654.3 % Show Supplier Material materials with Dehnung of 654.3 % | ASTM D412 | 500 mm/min | |
Druckverformungsrest | 23 °C | 20.6 [-] Show Supplier Material materials with Druckverformungsrest of 20.6 [-] | ASTM D395 B | |
70 °C | 62 [-] Show Supplier Material materials with Druckverformungsrest of 62 [-] | ASTM D395 B | ||
Härte, Shore A | 47 - 53 [-] Show Supplier Material materials with Härte, Shore A of 47 - 53 [-] | ASTM D2240 | ||
Modul bei 100 % Dehnung | 0.00119 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.00119 GPa | ASTM D412 | 500 mm/min | |
Modul bei 300 % Dehnung | 0.00178 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.00178 GPa | ASTM D412 | 500 mm/min | |
Reißfestigkeit | 15.8 kN/m Show Supplier Material materials with Reißfestigkeit of 15.8 kN/m | ASTM D624 Die C | 500 mm/min | |
Zugfestigkeit | 3.0 MPa Show Supplier Material materials with Zugfestigkeit of 3.0 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 6.9 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 6.9 g/10min | ASTM D1238 | 190°C/1.2kg |
Schrumpfung | 0.6 - 1.2 % Show Supplier Material materials with Schrumpfung of 0.6 - 1.2 % | ASTM D955 | Transverse |
1.2 - 1.8 % Show Supplier Material materials with Schrumpfung of 1.2 - 1.8 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Bicycle grip, golf club grip, tool grip, toothbrush, diving flipper, nasal aspirator | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3, Meets FDA requirements | |
Color | White | |
Fillers | Calcium Carbonate | |
Other | Overmolding capabilities: PP |