Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 1.15 - 1.21 g/cm³ Show Supplier Material materials with Dichte of 1.15 - 1.21 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dehnung | 703.5 % Show Supplier Material materials with Dehnung of 703.5 % | ASTM D412 | 500 mm/min |
Härte, Shore A | 47 - 53 [-] Show Supplier Material materials with Härte, Shore A of 47 - 53 [-] | ASTM D2240 | |
Modul bei 100 % Dehnung | 0.00102 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.00102 GPa | ASTM D412 | 500 mm/min |
Modul bei 300 % Dehnung | 0.00172 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.00172 GPa | ASTM D412 | 500 mm/min |
Reißfestigkeit | 18.4 kN/m Show Supplier Material materials with Reißfestigkeit of 18.4 kN/m | ASTM D624 Die C | 500 mm/min |
Zugfestigkeit | 4.4 MPa Show Supplier Material materials with Zugfestigkeit of 4.4 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 6.7 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 6.7 g/10min | ASTM D1238 | 200°C/5kg |
Schrumpfung | 1.1 - 1.7 % Show Supplier Material materials with Schrumpfung of 1.1 - 1.7 % | ASTM D955 | Transverse |
1.5 - 2.1 % Show Supplier Material materials with Schrumpfung of 1.5 - 2.1 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Bicycle grip, tool grip, hanger clip pad | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | White | |
Fillers | Calcium Carbonate | |
Other | Overmolding capabilities: PP |