Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 1.05 - 1.11 g/cm³ Show Supplier Material materials with Dichte of 1.05 - 1.11 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 824 % Show Supplier Material materials with Dehnung of 824 % | ASTM D412 | 500 mm/min | |
Druckverformungsrest | 23 °C | 22.7 [-] Show Supplier Material materials with Druckverformungsrest of 22.7 [-] | ASTM D395 B | |
70 °C | 51.3 [-] Show Supplier Material materials with Druckverformungsrest of 51.3 [-] | ASTM D395 B | ||
Härte, Shore A | 52 - 58 [-] Show Supplier Material materials with Härte, Shore A of 52 - 58 [-] | ASTM D2240 | ||
Modul bei 100 % Dehnung | 0.00148 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.00148 GPa | ASTM D412 | 500 mm/min | |
Modul bei 300 % Dehnung | 0.00204 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.00204 GPa | ASTM D412 | 500 mm/min | |
Reißfestigkeit | 20.4 kN/m Show Supplier Material materials with Reißfestigkeit of 20.4 kN/m | ASTM D624 Die C | 500 mm/min | |
Zugfestigkeit | 5.5 MPa Show Supplier Material materials with Zugfestigkeit of 5.5 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 11.1 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 11.1 g/10min | ASTM D1238 | 190°C/2.16kg |
Schrumpfung | 0.6 - 1.2 % Show Supplier Material materials with Schrumpfung of 0.6 - 1.2 % | ASTM D955 | Transverse |
0.7 - 1.3 % Show Supplier Material materials with Schrumpfung of 0.7 - 1.3 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Bicycle grip, golf club grip, tool grip, toothbrush, diving flipper, container seal | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3, Meets FDA requirements | |
Color | White | |
Fillers | Calcium Carbonate | |
Other | Overmolding capabilities: PP |