Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 1.03 - 1.09 g/cm³ Show Supplier Material materials with Dichte of 1.03 - 1.09 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 948.8 % Show Supplier Material materials with Dehnung of 948.8 % | ASTM D412 | 500 mm/min | |
Druckverformungsrest | 23 °C | 19.1 [-] Show Supplier Material materials with Druckverformungsrest of 19.1 [-] | ASTM D395 B | |
70 °C | 52.6 [-] Show Supplier Material materials with Druckverformungsrest of 52.6 [-] | ASTM D395 B | ||
Härte, Shore A | 57 - 63 [-] Show Supplier Material materials with Härte, Shore A of 57 - 63 [-] | ASTM D2240 | ||
Modul bei 100 % Dehnung | 0.00148 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.00148 GPa | ASTM D412 | 500 mm/min | |
Modul bei 300 % Dehnung | 0.00196 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.00196 GPa | ASTM D412 | 500 mm/min | |
Reißfestigkeit | 22.1 kN/m Show Supplier Material materials with Reißfestigkeit of 22.1 kN/m | ASTM D624 Die C | 500 mm/min | |
Zugfestigkeit | 5.4 MPa Show Supplier Material materials with Zugfestigkeit of 5.4 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 5.4 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 5.4 g/10min | ASTM D1238 | 190°C/2.16kg |
Schrumpfung | 0.8 - 1.4 % Show Supplier Material materials with Schrumpfung of 0.8 - 1.4 % | ASTM D955 | Transverse |
0.9 - 1.5 % Show Supplier Material materials with Schrumpfung of 0.9 - 1.5 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Bottle grip, cosmetics | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | White | |
Fillers | Calcium Carbonate | |
Other | Overmolding capabilities: PP, PE |