Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 1.06 - 1.12 g/cm³ Show Supplier Material materials with Dichte of 1.06 - 1.12 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 412.8 % Show Supplier Material materials with Dehnung of 412.8 % | ASTM D412 | 500 mm/min | |
Druckverformungsrest | 23 °C | 14.5 [-] Show Supplier Material materials with Druckverformungsrest of 14.5 [-] | ASTM D395 B | |
70 °C | 88.2 [-] Show Supplier Material materials with Druckverformungsrest of 88.2 [-] | ASTM D395 B | ||
Härte, Shore A | 47 - 53 [-] Show Supplier Material materials with Härte, Shore A of 47 - 53 [-] | ASTM D2240 | ||
Modul bei 100 % Dehnung | 0.00105 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.00105 GPa | ASTM D412 | 500 mm/min | |
Modul bei 300 % Dehnung | 0.00165 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.00165 GPa | ASTM D412 | 500 mm/min | |
Reißfestigkeit | 11.1 kN/m Show Supplier Material materials with Reißfestigkeit of 11.1 kN/m | ASTM D624 Die C | 500 mm/min | |
Zugfestigkeit | 2.0 MPa Show Supplier Material materials with Zugfestigkeit of 2.0 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 31.5 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 31.5 g/10min | ASTM D1238 | 190°C/2.16kg |
Schrumpfung | 1.1 - 1.7 % Show Supplier Material materials with Schrumpfung of 1.1 - 1.7 % | ASTM D955 | Transverse |
1.2 - 1.8 % Show Supplier Material materials with Schrumpfung of 1.2 - 1.8 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Tool grip, toothbrush, non-slip mat, buttons and knobs, pen grip | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3, Meets FDA requirements | |
Color | White | |
Fillers | Calcium Carbonate | |
Other | Overmolding capabilities: PP |