Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 1.03 - 1.09 g/cm³ Show Supplier Material materials with Dichte of 1.03 - 1.09 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dehnung | 253.6 % Show Supplier Material materials with Dehnung of 253.6 % | ASTM D412 | 500 mm/min |
Härte, Shore A | 62 - 68 [-] Show Supplier Material materials with Härte, Shore A of 62 - 68 [-] | ASTM D2240 | |
Modul bei 100 % Dehnung | 0.00183 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.00183 GPa | ASTM D412 | 500 mm/min |
Reißfestigkeit | 13.1 kN/m Show Supplier Material materials with Reißfestigkeit of 13.1 kN/m | ASTM D624 Die C | 500 mm/min |
Zugfestigkeit | 2.3 MPa Show Supplier Material materials with Zugfestigkeit of 2.3 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 33.1 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 33.1 g/10min | ASTM D1238 | 190°C/2.16kg |
Schrumpfung | 0.8 - 1.4 % Show Supplier Material materials with Schrumpfung of 0.8 - 1.4 % | ASTM D955 | Transverse |
0.9 - 1.5 % Show Supplier Material materials with Schrumpfung of 0.9 - 1.5 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Bicycle grip, tool grip, pen grip, toothbrush | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | White | |
Fillers | Calcium Carbonate | |
Other | Overmolding capabilities: PP |