Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 1.19 - 1.25 g/cm³ Show Supplier Material materials with Dichte of 1.19 - 1.25 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dehnung | 577.6 % Show Supplier Material materials with Dehnung of 577.6 % | ASTM D412 | 500 mm/min |
Härte, Shore A | 57 - 63 [-] Show Supplier Material materials with Härte, Shore A of 57 - 63 [-] | ASTM D2240 | |
Modul bei 100 % Dehnung | 0.0025 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.0025 GPa | ASTM D412 | 500 mm/min |
Modul bei 300 % Dehnung | 0.00403 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.00403 GPa | ASTM D412 | 500 mm/min |
Reißfestigkeit | 33.4 kN/m Show Supplier Material materials with Reißfestigkeit of 33.4 kN/m | ASTM D624 Die C | 500 mm/min |
Zugfestigkeit | 7.8 MPa Show Supplier Material materials with Zugfestigkeit of 7.8 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 36.9 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 36.9 g/10min | ASTM D1238 | 200°C/5kg |
Schrumpfung | 1.1 - 1.7 % Show Supplier Material materials with Schrumpfung of 1.1 - 1.7 % | ASTM D955 | Transverse |
1.3 - 1.9 % Show Supplier Material materials with Schrumpfung of 1.3 - 1.9 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Electrical and pneumatic tool grip, electronic appliances, tool grip | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | White | |
Fillers | Calcium Carbonate | |
Other | Overmolding capabilities: ABS, AS, PMMA, PA |