Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 1.03 - 1.09 g/cm³ Show Supplier Material materials with Dichte of 1.03 - 1.09 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dehnung | 493.6 % Show Supplier Material materials with Dehnung of 493.6 % | ASTM D412 | 500 mm/min |
Härte, Shore A | 62 - 68 [-] Show Supplier Material materials with Härte, Shore A of 62 - 68 [-] | ASTM D2240 | |
Modul bei 100 % Dehnung | 0.00286 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.00286 GPa | ASTM D412 | 500 mm/min |
Modul bei 300 % Dehnung | 0.0049 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.0049 GPa | ASTM D412 | 500 mm/min |
Reißfestigkeit | 35.1 kN/m Show Supplier Material materials with Reißfestigkeit of 35.1 kN/m | ASTM D624 Die C | 500 mm/min |
Zugfestigkeit | 10.1 MPa Show Supplier Material materials with Zugfestigkeit of 10.1 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 23.1 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 23.1 g/10min | ASTM D1238 | 200°C/5kg |
Schrumpfung | 0.8 - 1.4 % Show Supplier Material materials with Schrumpfung of 0.8 - 1.4 % | ASTM D955 | Transverse |
0.9 - 1.5 % Show Supplier Material materials with Schrumpfung of 0.9 - 1.5 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Electrical and pneumatic tool grip, electronic appliances, tool grip | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | White | |
Fillers | Calcium Carbonate | |
Other | Overmolding capabilities: ABS, AS, PET-G, PMMA, PCTG |