Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 1 - 1.06 g/cm³ Show Supplier Material materials with Dichte of 1 - 1.06 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dehnung | 711.4 % Show Supplier Material materials with Dehnung of 711.4 % | ASTM D412 | 500 mm/min |
Härte, Shore A | 67 - 73 [-] Show Supplier Material materials with Härte, Shore A of 67 - 73 [-] | ASTM D2240 | |
Modul bei 100 % Dehnung | 0.00201 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.00201 GPa | ASTM D412 | 500 mm/min |
Modul bei 300 % Dehnung | 0.00341 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.00341 GPa | ASTM D412 | 500 mm/min |
Reißfestigkeit | 34.4 kN/m Show Supplier Material materials with Reißfestigkeit of 34.4 kN/m | ASTM D624 Die C | 500 mm/min |
Zugfestigkeit | 9.0 MPa Show Supplier Material materials with Zugfestigkeit of 9.0 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 0.8 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 0.8 g/10min | ASTM D1238 | 200°C/5kg |
Schrumpfung | 1.4 - 2 % Show Supplier Material materials with Schrumpfung of 1.4 - 2 % | ASTM D955 | Transverse |
1.5 - 2.1 % Show Supplier Material materials with Schrumpfung of 1.5 - 2.1 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Extrusion profile, weather seal | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | Black | |
Fillers | Calcium Carbonate | |
Other | Overmolding capabilities: PP |