Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 0.94 - 1 g/cm³ Show Supplier Material materials with Dichte of 0.94 - 1 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 798.8 % Show Supplier Material materials with Dehnung of 798.8 % | ASTM D412 | 500 mm/min | |
Druckverformungsrest | 23 °C | 25.3 [-] Show Supplier Material materials with Druckverformungsrest of 25.3 [-] | ASTM D395 B | |
70 °C | 45.9 [-] Show Supplier Material materials with Druckverformungsrest of 45.9 [-] | ASTM D395 B | ||
Härte, Shore A | 77 - 83 [-] Show Supplier Material materials with Härte, Shore A of 77 - 83 [-] | ASTM D2240 | ||
Modul bei 100 % Dehnung | 0.0029 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.0029 GPa | ASTM D412 | 500 mm/min | |
Modul bei 300 % Dehnung | 0.00413 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.00413 GPa | ASTM D412 | 500 mm/min | |
Reißfestigkeit | 42.7 kN/m Show Supplier Material materials with Reißfestigkeit of 42.7 kN/m | ASTM D624 Die C | 500 mm/min | |
Zugfestigkeit | 10.3 MPa Show Supplier Material materials with Zugfestigkeit of 10.3 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 1.5 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 1.5 g/10min | ASTM D1238 | 200°C/5kg |
Schrumpfung | 1.2 - 1.8 % Show Supplier Material materials with Schrumpfung of 1.2 - 1.8 % | ASTM D955 | |
1.2 - 1.8 % Show Supplier Material materials with Schrumpfung of 1.2 - 1.8 % | ASTM D955 | Transverse |
Technological properties
Property | ||
---|---|---|
Application areas | Pipe seal, valve seal | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | Natural | |
Fillers | Calcium Carbonate | |
Other | Overmolding capabilities: PP |