Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 0.9 - 0.96 g/cm³ Show Supplier Material materials with Dichte of 0.9 - 0.96 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dehnung | 856.1 % Show Supplier Material materials with Dehnung of 856.1 % | ASTM D412 | 500 mm/min |
Härte, Shore A | 87 - 93 [-] Show Supplier Material materials with Härte, Shore A of 87 - 93 [-] | ASTM D2240 | |
Modul bei 100 % Dehnung | 0.00623 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.00623 GPa | ASTM D412 | 500 mm/min |
Modul bei 300 % Dehnung | 0.00599 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.00599 GPa | ASTM D412 | 500 mm/min |
Reißfestigkeit | 68.0 kN/m Show Supplier Material materials with Reißfestigkeit of 68.0 kN/m | ASTM D624 Die C | 500 mm/min |
Zugfestigkeit | 10.4 MPa Show Supplier Material materials with Zugfestigkeit of 10.4 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 14.2 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 14.2 g/10min | ASTM D1238 | 190°C/2.16kg |
Schrumpfung | 0.5 - 1.1 % Show Supplier Material materials with Schrumpfung of 0.5 - 1.1 % | ASTM D955 | Transverse |
0.6 - 1.2 % Show Supplier Material materials with Schrumpfung of 0.6 - 1.2 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Car carpet | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | Natural | |
Other | Overmolding capabilities: PP |