Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 1.03 - 1.09 g/cm³ Show Supplier Material materials with Dichte of 1.03 - 1.09 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dehnung | 209.6 % Show Supplier Material materials with Dehnung of 209.6 % | ASTM D412 | 500 mm/min |
Härte, Shore A | 57 - 63 [-] Show Supplier Material materials with Härte, Shore A of 57 - 63 [-] | ASTM D2240 | |
Modul bei 100 % Dehnung | 0.00165 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.00165 GPa | ASTM D412 | 500 mm/min |
Reißfestigkeit | 11.8 kN/m Show Supplier Material materials with Reißfestigkeit of 11.8 kN/m | ASTM D624 Die C | 500 mm/min |
Zugfestigkeit | 2.0 MPa Show Supplier Material materials with Zugfestigkeit of 2.0 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 25.9 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 25.9 g/10min | ASTM D1238 | 190°C/2.16kg |
Schrumpfung | 1.1 - 1.7 % Show Supplier Material materials with Schrumpfung of 1.1 - 1.7 % | ASTM D955 | Transverse |
1.2 - 1.8 % Show Supplier Material materials with Schrumpfung of 1.2 - 1.8 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Tool grip, buttons and knobs, toys | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | Black | |
Fillers | Calcium Carbonate | |
Other | Overmolding capabilities: PP |