Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 0.85 - 0.91 g/cm³ Show Supplier Material materials with Dichte of 0.85 - 0.91 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 559.6 % Show Supplier Material materials with Dehnung of 559.6 % | ASTM D412 | 500 mm/min | |
Druckverformungsrest | 23 °C | 36.5 [-] Show Supplier Material materials with Druckverformungsrest of 36.5 [-] | ASTM D395 B | |
70 °C | 67.3 [-] Show Supplier Material materials with Druckverformungsrest of 67.3 [-] | ASTM D395 B | ||
Härte, Shore A | 72 - 78 [-] Show Supplier Material materials with Härte, Shore A of 72 - 78 [-] | ASTM D2240 | ||
Modul bei 100 % Dehnung | 0.00335 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.00335 GPa | ASTM D412 | 500 mm/min | |
Modul bei 300 % Dehnung | 0.00422 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.00422 GPa | ASTM D412 | 500 mm/min | |
Reißfestigkeit | 31.4 kN/m Show Supplier Material materials with Reißfestigkeit of 31.4 kN/m | ASTM D624 Die C | 500 mm/min | |
Zugfestigkeit | 5.5 MPa Show Supplier Material materials with Zugfestigkeit of 5.5 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 42 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 42 g/10min | ASTM D1238 | 190°C/2.16kg |
Schrumpfung | 1.2 - 1.8 % Show Supplier Material materials with Schrumpfung of 1.2 - 1.8 % | ASTM D955 | Transverse |
2.3 - 2.9 % Show Supplier Material materials with Schrumpfung of 2.3 - 2.9 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Medical appliances, tool grip, toothbrush, pen grip | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3, Meets FDA requirements | |
Color | Translucent | |
Other | Overmolding capabilities: PP |