Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 0.84 - 0.9 g/cm³ Show Supplier Material materials with Dichte of 0.84 - 0.9 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 698 % Show Supplier Material materials with Dehnung of 698 % | ASTM D412 | 500 mm/min | |
Druckverformungsrest | 23 °C | 29.9 [-] Show Supplier Material materials with Druckverformungsrest of 29.9 [-] | ASTM D395 B | |
70 °C | 63.9 [-] Show Supplier Material materials with Druckverformungsrest of 63.9 [-] | ASTM D395 B | ||
Härte, Shore A | 77 - 83 [-] Show Supplier Material materials with Härte, Shore A of 77 - 83 [-] | ASTM D2240 | ||
Modul bei 100 % Dehnung | 0.00417 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.00417 GPa | ASTM D412 | 500 mm/min | |
Modul bei 300 % Dehnung | 0.00503 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.00503 GPa | ASTM D412 | 500 mm/min | |
Reißfestigkeit | 42 kN/m Show Supplier Material materials with Reißfestigkeit of 42 kN/m | ASTM D624 Die C | 500 mm/min | |
Zugfestigkeit | 8.0 MPa Show Supplier Material materials with Zugfestigkeit of 8.0 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 37 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 37 g/10min | ASTM D1238 | 190°C/2.16kg |
Schrumpfung | 1 - 1.6 % Show Supplier Material materials with Schrumpfung of 1 - 1.6 % | ASTM D955 | |
1 - 1.6 % Show Supplier Material materials with Schrumpfung of 1 - 1.6 % | ASTM D955 | Transverse |
Technological properties
Property | ||
---|---|---|
Application areas | Medical appliances, tool grip, toothbrush, pen grip | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3, Meets FDA requirements | |
Color | Translucent | |
Other | Overmolding capabilities: PP |