Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 0.85 - 0.91 g/cm³ Show Supplier Material materials with Dichte of 0.85 - 0.91 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 807.3 % Show Supplier Material materials with Dehnung of 807.3 % | ASTM D412 | 500 mm/min | |
Druckverformungsrest | 23 °C | 36.7 [-] Show Supplier Material materials with Druckverformungsrest of 36.7 [-] | ASTM D395 B | |
70 °C | 63 [-] Show Supplier Material materials with Druckverformungsrest of 63 [-] | ASTM D395 B | ||
Härte, Shore A | 82 - 88 [-] Show Supplier Material materials with Härte, Shore A of 82 - 88 [-] | ASTM D2240 | ||
Modul bei 100 % Dehnung | 0.00537 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.00537 GPa | ASTM D412 | 500 mm/min | |
Modul bei 300 % Dehnung | 0.00613 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.00613 GPa | ASTM D412 | 500 mm/min | |
Reißfestigkeit | 56.2 kN/m Show Supplier Material materials with Reißfestigkeit of 56.2 kN/m | ASTM D624 Die C | 500 mm/min | |
Zugfestigkeit | 11.8 MPa Show Supplier Material materials with Zugfestigkeit of 11.8 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 28.4 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 28.4 g/10min | ASTM D1238 | 190°C/2.16kg |
Schrumpfung | 1 - 1.6 % Show Supplier Material materials with Schrumpfung of 1 - 1.6 % | ASTM D955 | |
1 - 1.6 % Show Supplier Material materials with Schrumpfung of 1 - 1.6 % | ASTM D955 | Transverse |
Technological properties
Property | ||
---|---|---|
Application areas | Medical appliances, tool grip | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3, Meets FDA requirements | |
Color | Translucent | |
Other | Overmolding capabilities: PP |