Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 0.85 - 0.91 g/cm³ Show Supplier Material materials with Dichte of 0.85 - 0.91 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 703.9 % Show Supplier Material materials with Dehnung of 703.9 % | ASTM D412 | 500 mm/min | |
Druckverformungsrest | 70 °C | 59.4 [-] Show Supplier Material materials with Druckverformungsrest of 59.4 [-] | ASTM D395 B | |
Härte, Shore A | 72 - 78 [-] Show Supplier Material materials with Härte, Shore A of 72 - 78 [-] | ASTM D2240 | ||
Modul bei 100 % Dehnung | 0.0027 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.0027 GPa | ASTM D412 | 500 mm/min | |
Modul bei 300 % Dehnung | 0.00367 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.00367 GPa | ASTM D412 | 500 mm/min | |
Reißfestigkeit | 33.3 kN/m Show Supplier Material materials with Reißfestigkeit of 33.3 kN/m | ASTM D624 Die C | 500 mm/min | |
Zugfestigkeit | 6.9 MPa Show Supplier Material materials with Zugfestigkeit of 6.9 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 171 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 171 g/10min | ASTM D1238 | 190°C/5kg |
Schrumpfung | 0.9 - 1.5 % Show Supplier Material materials with Schrumpfung of 0.9 - 1.5 % | ASTM D955 | Transverse |
1.1 - 1.7 % Show Supplier Material materials with Schrumpfung of 1.1 - 1.7 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Caster wheel, pen grip, seal | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3, Meets FDA requirements, Bio-Compatible | |
Color | Translucent | |
Other | Overmolding capabilities: PP |