Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 0.85 - 0.91 g/cm³ Show Supplier Material materials with Dichte of 0.85 - 0.91 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 763.2 % Show Supplier Material materials with Dehnung of 763.2 % | ASTM D412 | 500 mm/min | |
Druckverformungsrest | 23 °C | 30.6 [-] Show Supplier Material materials with Druckverformungsrest of 30.6 [-] | ASTM D395 B | |
70 °C | 53.8 [-] Show Supplier Material materials with Druckverformungsrest of 53.8 [-] | ASTM D395 B | ||
Härte, Shore A | 87 - 93 [-] Show Supplier Material materials with Härte, Shore A of 87 - 93 [-] | ASTM D2240 | ||
Modul bei 100 % Dehnung | 0.00579 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.00579 GPa | ASTM D412 | 500 mm/min | |
Modul bei 300 % Dehnung | 0.00723 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.00723 GPa | ASTM D412 | 500 mm/min | |
Reißfestigkeit | 73.1 kN/m Show Supplier Material materials with Reißfestigkeit of 73.1 kN/m | ASTM D624 Die C | 500 mm/min | |
Zugfestigkeit | 18.5 MPa Show Supplier Material materials with Zugfestigkeit of 18.5 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 9.7 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 9.7 g/10min | ASTM D1238 | 190°C/5kg |
Schrumpfung | 1.1 - 1.7 % Show Supplier Material materials with Schrumpfung of 1.1 - 1.7 % | ASTM D955 | Transverse |
1.3 - 1.9 % Show Supplier Material materials with Schrumpfung of 1.3 - 1.9 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive interior | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | Translucent | |
Other | Overmolding capabilities: PP |