Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 1.27 - 1.33 g/cm³ Show Supplier Material materials with Dichte of 1.27 - 1.33 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dehnung | 821.2 % Show Supplier Material materials with Dehnung of 821.2 % | ASTM D412 | 500 mm/min |
Härte, Shore A | 27 - 33 [-] Show Supplier Material materials with Härte, Shore A of 27 - 33 [-] | ASTM D2240 | |
Modul bei 100 % Dehnung | 0.00044 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.00044 GPa | ASTM D412 | 500 mm/min |
Modul bei 300 % Dehnung | 0.00067 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.00067 GPa | ASTM D412 | 500 mm/min |
Reißfestigkeit | 9.0 kN/m Show Supplier Material materials with Reißfestigkeit of 9.0 kN/m | ASTM D624 Die C | 500 mm/min |
Zugfestigkeit | 2.0 MPa Show Supplier Material materials with Zugfestigkeit of 2.0 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 13.9 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 13.9 g/10min | ASTM D1238 | 190°C/2.16kg |
Schrumpfung | 1.4 - 2 % Show Supplier Material materials with Schrumpfung of 1.4 - 2 % | ASTM D955 | Transverse |
1.5 - 2.1 % Show Supplier Material materials with Schrumpfung of 1.5 - 2.1 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Toothbrush and many more… | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | White | |
Fillers | Calcium Carbonate | |
Other | Overmolding capabilities: PP | |
Processing methods |