Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 0.86 - 0.92 g/cm³ Show Supplier Material materials with Dichte of 0.86 - 0.92 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dehnung | 711.6 % Show Supplier Material materials with Dehnung of 711.6 % | ASTM D412 | 500 mm/min |
Härte, Shore A | 72 - 78 [-] Show Supplier Material materials with Härte, Shore A of 72 - 78 [-] | ASTM D2240 | |
Modul bei 100 % Dehnung | 0.00278 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.00278 GPa | ASTM D412 | 500 mm/min |
Modul bei 300 % Dehnung | 0.00404 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.00404 GPa | ASTM D412 | 500 mm/min |
Reißfestigkeit | 38.4 kN/m Show Supplier Material materials with Reißfestigkeit of 38.4 kN/m | ASTM D624 Die C | 500 mm/min |
Zugfestigkeit | 7.4 MPa Show Supplier Material materials with Zugfestigkeit of 7.4 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 9.9 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 9.9 g/10min | ASTM D1238 | 200°C/5kg |
Schrumpfung | 1.1 - 1.7 % Show Supplier Material materials with Schrumpfung of 1.1 - 1.7 % | ASTM D955 | Transverse |
1.2 - 1.8 % Show Supplier Material materials with Schrumpfung of 1.2 - 1.8 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Extrusion profile, weather seal and many more… | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | Natural | |
Other | Overmolding capabilities: PP | |
Processing methods |