Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 1.03 - 1.09 g/cm³ Show Supplier Material materials with Dichte of 1.03 - 1.09 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dehnung | 573 % Show Supplier Material materials with Dehnung of 573 % | ASTM D412 | 500 mm/min |
Härte, Shore A | 77 - 83 [-] Show Supplier Material materials with Härte, Shore A of 77 - 83 [-] | ASTM D2240 | |
Modul bei 100 % Dehnung | 0.00402 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.00402 GPa | ASTM D412 | 500 mm/min |
Modul bei 300 % Dehnung | 0.00507 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.00507 GPa | ASTM D412 | 500 mm/min |
Reißfestigkeit | 42.0 kN/m Show Supplier Material materials with Reißfestigkeit of 42.0 kN/m | ASTM D624 Die C | 500 mm/min |
Zugfestigkeit | 7.2 MPa Show Supplier Material materials with Zugfestigkeit of 7.2 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 32.1 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 32.1 g/10min | ASTM D1238 | 190°C/2.16kg |
Schrumpfung | 0.8 - 1.4 % Show Supplier Material materials with Schrumpfung of 0.8 - 1.4 % | ASTM D955 | |
0.8 - 1.4 % Show Supplier Material materials with Schrumpfung of 0.8 - 1.4 % | ASTM D955 | Transverse |
Technological properties
Property | ||
---|---|---|
Application areas | Battery cover seal and many more… | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | Black | |
Fillers | Calcium Carbonate | |
Other | Overmolding capabilities: PP | |
Processing methods |