Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 0.85 - 0.91 g/cm³ Show Supplier Material materials with Dichte of 0.85 - 0.91 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dehnung | 805.6 % Show Supplier Material materials with Dehnung of 805.6 % | ASTM D412 | 500 mm/min |
Härte, Shore A | 52 - 58 [-] Show Supplier Material materials with Härte, Shore A of 52 - 58 [-] | ASTM D2240 | |
Modul bei 100 % Dehnung | 0.00075 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.00075 GPa | ASTM D412 | 500 mm/min |
Modul bei 300 % Dehnung | 0.00148 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.00148 GPa | ASTM D412 | 500 mm/min |
Reißfestigkeit | 19.4 kN/m Show Supplier Material materials with Reißfestigkeit of 19.4 kN/m | ASTM D624 Die C | 500 mm/min |
Zugfestigkeit | 4.9 MPa Show Supplier Material materials with Zugfestigkeit of 4.9 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 8.8 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 8.8 g/10min | ASTM D1238 | 190°C/5kg |
Schrumpfung | 1.3 - 1.9 % Show Supplier Material materials with Schrumpfung of 1.3 - 1.9 % | ASTM D955 | Transverse |
1.5 - 2.1 % Show Supplier Material materials with Schrumpfung of 1.5 - 2.1 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Extrusion profile, tube, sports equipment and many more… | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3, Meets FDA requirements, Bio-Compatible | |
Color | Translucent | |
Other | Overmolding capabilities: PP | |
Processing methods |