Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 0.84 - 0.9 g/cm³ Show Supplier Material materials with Dichte of 0.84 - 0.9 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dehnung | 998.5 % Show Supplier Material materials with Dehnung of 998.5 % | ASTM D412 | 500 mm/min |
Härte, Shore A | 44548 [-] Show Supplier Material materials with Härte, Shore A of 44548 [-] | ASTM D2240 | |
Modul bei 100 % Dehnung | 0.00028 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.00028 GPa | ASTM D412 | 500 mm/min |
Modul bei 300 % Dehnung | 0.00057 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.00057 GPa | ASTM D412 | 500 mm/min |
Reißfestigkeit | 13.0 kN/m Show Supplier Material materials with Reißfestigkeit of 13.0 kN/m | ASTM D624 Die C | 500 mm/min |
Zugfestigkeit | 3.2 MPa Show Supplier Material materials with Zugfestigkeit of 3.2 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 161.3 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 161.3 g/10min | ASTM D1238 | 190°C/5kg |
Schrumpfung | 1.6 - 2.2 % Show Supplier Material materials with Schrumpfung of 1.6 - 2.2 % | ASTM D955 | Transverse |
2.3 - 2.9 % Show Supplier Material materials with Schrumpfung of 2.3 - 2.9 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Pad brush and many more… | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | Translucent | |
Other | Overmolding capabilities: PP | |
Processing methods |