Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 0.85 - 0.91 g/cm³ Show Supplier Material materials with Dichte of 0.85 - 0.91 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dehnung | 427 % Show Supplier Material materials with Dehnung of 427 % | ASTM D412 | 500 mm/min |
Härte, Shore A | 82 - 88 [-] Show Supplier Material materials with Härte, Shore A of 82 - 88 [-] | ASTM D2240 | |
Modul bei 100 % Dehnung | 0.0042 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.0042 GPa | ASTM D412 | 500 mm/min |
Modul bei 300 % Dehnung | 0.0049 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.0049 GPa | ASTM D412 | 500 mm/min |
Reißfestigkeit | 31.9 kN/m Show Supplier Material materials with Reißfestigkeit of 31.9 kN/m | ASTM D624 Die C | 500 mm/min |
Zugfestigkeit | 5.3 MPa Show Supplier Material materials with Zugfestigkeit of 5.3 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 41.4 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 41.4 g/10min | ASTM D1238 | 190°C/2.16kg |
Schrumpfung | 0.6 - 1.2 % Show Supplier Material materials with Schrumpfung of 0.6 - 1.2 % | ASTM D955 | Transverse |
0.8 - 1.4 % Show Supplier Material materials with Schrumpfung of 0.8 - 1.4 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Medical appliance, tool grip, and many more… | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3, Meets FDA requirements | |
Color | Translucent | |
Other | Overmolding capabilities: PP | |
Processing methods |