Allgemein
Property | Value | Testing Standard | |
---|---|---|---|
Dichte | 1.14 - 1.2 g/cm³ Show Supplier Material materials with Dichte of 1.14 - 1.2 g/cm³ | ASTM D792 | |
Recycled Content | 30-40 |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dehnung | 831 % Show Supplier Material materials with Dehnung of 831 % | ASTM D412 | 500 mm/min |
Härte, Shore A | 42 - 48 [-] Show Supplier Material materials with Härte, Shore A of 42 - 48 [-] | ASTM D2240 | |
Modul bei 100 % Dehnung | 0.00077 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.00077 GPa | ASTM D412 | 500 mm/min |
Modul bei 300 % Dehnung | 0.0011 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.0011 GPa | ASTM D412 | 500 mm/min |
Reißfestigkeit | 13.0 kN/m Show Supplier Material materials with Reißfestigkeit of 13.0 kN/m | ASTM D624 Die C | 500 mm/min |
Zugfestigkeit | 2.5 MPa Show Supplier Material materials with Zugfestigkeit of 2.5 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 16.2 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 16.2 g/10min | ASTM D1238 | 190°C/2.16kg |
Schrumpfung | 0.6 - 1.2 % Show Supplier Material materials with Schrumpfung of 0.6 - 1.2 % | ASTM D955 | Transverse |
0.7 - 1.3 % Show Supplier Material materials with Schrumpfung of 0.7 - 1.3 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | PP Modifier, Grip, Sports and mamy more... | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | Black | |
Other | Overmolding capabilities: PP | |
Processing methods |