Allgemein
Property | Value | Testing Standard | |
---|---|---|---|
Dichte | 1.16 - 1.22 g/cm³ Show Supplier Material materials with Dichte of 1.16 - 1.22 g/cm³ | ASTM D792 | |
Recycled Content | 25-35 |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dehnung | 785.2 % Show Supplier Material materials with Dehnung of 785.2 % | ASTM D412 | 500 mm/min |
Härte, Shore A | 47 - 53 [-] Show Supplier Material materials with Härte, Shore A of 47 - 53 [-] | ASTM D2240 | |
Modul bei 100 % Dehnung | 0.00082 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.00082 GPa | ASTM D412 | 500 mm/min |
Modul bei 300 % Dehnung | 0.0012 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.0012 GPa | ASTM D412 | 500 mm/min |
Reißfestigkeit | 11.3 kN/m Show Supplier Material materials with Reißfestigkeit of 11.3 kN/m | ASTM D624 Die C | 500 mm/min |
Zugfestigkeit | 2.2 MPa Show Supplier Material materials with Zugfestigkeit of 2.2 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 23.6 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 23.6 g/10min | ASTM D1238 | 190°C/2.16kg |
Schrumpfung | 0.8 - 1.4 % Show Supplier Material materials with Schrumpfung of 0.8 - 1.4 % | ASTM D955 | Transverse |
1 - 1.6 % Show Supplier Material materials with Schrumpfung of 1 - 1.6 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Electrical boot and many more... | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | Black | |
Processing methods |