Allgemein
Property | Value | Testing Standard | |
---|---|---|---|
Dichte | 1.11 - 1.17 g/cm³ Show Supplier Material materials with Dichte of 1.11 - 1.17 g/cm³ | ASTM D792 | |
Recycled Content | 30-40 |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dehnung | 550.5 % Show Supplier Material materials with Dehnung of 550.5 % | ASTM D412 | 500 mm/min |
Härte, Shore A | 67 - 73 [-] Show Supplier Material materials with Härte, Shore A of 67 - 73 [-] | ASTM D2240 | |
Modul bei 100 % Dehnung | 0.0021 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.0021 GPa | ASTM D412 | 500 mm/min |
Modul bei 300 % Dehnung | 0.0027 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.0027 GPa | ASTM D412 | 500 mm/min |
Reißfestigkeit | 22.9 kN/m Show Supplier Material materials with Reißfestigkeit of 22.9 kN/m | ASTM D624 Die C | 500 mm/min |
Zugfestigkeit | 3.5 MPa Show Supplier Material materials with Zugfestigkeit of 3.5 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 20.2 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 20.2 g/10min | ASTM D1238 | 190°C/2.16kg |
Schrumpfung | 0.8 - 1.4 % Show Supplier Material materials with Schrumpfung of 0.8 - 1.4 % | ASTM D955 | Transverse |
0.9 - 1.5 % Show Supplier Material materials with Schrumpfung of 0.9 - 1.5 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Tool Grip and many more... | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | Black | |
Processing methods |