Allgemein
Property | Value | Testing Standard | |
---|---|---|---|
Dichte | 1.05 - 1.1 g/cm³ Show Supplier Material materials with Dichte of 1.05 - 1.1 g/cm³ | ASTM D792 | |
Recycled Content | 35-45 |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dehnung | 397.3 % Show Supplier Material materials with Dehnung of 397.3 % | ASTM D412 | 500 mm/min |
Härte, Shore A | 87 - 93 [-] Show Supplier Material materials with Härte, Shore A of 87 - 93 [-] | ASTM D2240 | |
Modul bei 100 % Dehnung | 0.0057 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.0057 GPa | ASTM D412 | 500 mm/min |
Modul bei 300 % Dehnung | 0.0063 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.0063 GPa | ASTM D412 | 500 mm/min |
Reißfestigkeit | 45.3 kN/m Show Supplier Material materials with Reißfestigkeit of 45.3 kN/m | ASTM D624 Die C | 500 mm/min |
Zugfestigkeit | 6.7 MPa Show Supplier Material materials with Zugfestigkeit of 6.7 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 17.6 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 17.6 g/10min | ASTM D1238 | 190°C/2.16kg |
Schrumpfung | 1.1 - 1.7 % Show Supplier Material materials with Schrumpfung of 1.1 - 1.7 % | ASTM D955 | Transverse |
1.5 - 2.1 % Show Supplier Material materials with Schrumpfung of 1.5 - 2.1 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Tool Grip and many more... | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | Black | |
Processing methods |