Allgemein
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Dichte | 1.66 g/cm³ Show Supplier Material materials with Dichte of 1.66 g/cm³ | dry | ISO 1183 | |||
Moisture absorption | 23 °C | 0.5 % Show Supplier Material materials with Moisture absorption of 0.5 % | 50%RH | ISO 62 | 2 mm | |
Wasserabsorption | 1.3 % Show Supplier Material materials with Wasserabsorption of 1.3 % | ISO 62 | 2 mm | immersion at 23°C |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Biegefestigkeit | 320 MPa Show Supplier Material materials with Biegefestigkeit of 320 MPa | 50%RH | ISO 178 | 2mm/min | |
340 MPa Show Supplier Material materials with Biegefestigkeit of 340 MPa | dry | ISO 178 | 2mm/min | ||
Biegemodul | 15.4 GPa Show Supplier Material materials with Biegemodul of 15.4 GPa | 50%RH | ISO 178 | 2mm/min | |
17 GPa Show Supplier Material materials with Biegemodul of 17 GPa | dry | ISO 178 | 2mm/min | ||
Dehnung | 2.9 % Show Supplier Material materials with Dehnung of 2.9 % | dry | ISO 527-2/1A | 5mm/min | |
3 % Show Supplier Material materials with Dehnung of 3 % | 50%RH | ISO 527-2/1A | 5mm/min | ||
Elastizitätsmodul | 17.2 GPa Show Supplier Material materials with Elastizitätsmodul of 17.2 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
19 GPa Show Supplier Material materials with Elastizitätsmodul of 19 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Schlagfestigkeit, Charpy gekerbt | 23 °C | 18 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 18 kJ/m² | dry | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | 23 °C | 100 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 100 kJ/m² | dry | ISO 179/1eU | |
23 °C | 105 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 105 kJ/m² | 50%RH | ISO 179/1eU | ||
Zugfestigkeit | 190 MPa Show Supplier Material materials with Zugfestigkeit of 190 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
220 MPa Show Supplier Material materials with Zugfestigkeit of 220 MPa | dry | ISO 527-2/1A | 5mm/min |
Thermisch
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | ISO 11357-1/-3 | 10°C/min | ||
Vicat-Erweichungstemperatur | 215 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 215 °C | ISO 306 | 1.00E+12mm | ||
Wärmeformbeständigkeitstemperatur | 190 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 190 °C | ISO 75/2Af | 8.00 MPa | ||
215 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 215 °C | ISO 75/2Af | 1.80 MPa | |||
Entflammbarkeit | Thickness tested (mm): 3, Class: HB, Standard: UL 94 |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schrumpfung | 0.2 % Show Supplier Material materials with Schrumpfung of 0.2 % | 280/90/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
0.3 % Show Supplier Material materials with Schrumpfung of 0.3 % | 280/90/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Fillers | 60% Glass Fiber | |
Processing methods | Injection Molding |