Allgemein
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Dichte | 1.59 g/cm³ Show Supplier Material materials with Dichte of 1.59 g/cm³ | dry | ISO 1183 | |||
Moisture absorption | 23 °C | 0.9 % Show Supplier Material materials with Moisture absorption of 0.9 % | 50%RH | ISO 62 | 2 mm | |
Wasserabsorption | 3.8 % Show Supplier Material materials with Wasserabsorption of 3.8 % | ISO 62 | 2 mm | immersion at 23°C |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Biegefestigkeit | 300 MPa Show Supplier Material materials with Biegefestigkeit of 300 MPa | 50%RH | ISO 178 | 2mm/min | |
375 MPa Show Supplier Material materials with Biegefestigkeit of 375 MPa | dry | ISO 178 | 2mm/min | ||
Biegemodul | 15.4 GPa Show Supplier Material materials with Biegemodul of 15.4 GPa | 50%RH | ISO 178 | 2mm/min | |
16.3 GPa Show Supplier Material materials with Biegemodul of 16.3 GPa | dry | ISO 178 | 2mm/min | ||
Dehnung | 2.3 % Show Supplier Material materials with Dehnung of 2.3 % | dry | ISO 527-2/1A | 5mm/min | |
3 % Show Supplier Material materials with Dehnung of 3 % | 50%RH | ISO 527-2/1A | 5mm/min | ||
Elastizitätsmodul | 14.6 GPa Show Supplier Material materials with Elastizitätsmodul of 14.6 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
17.6 GPa Show Supplier Material materials with Elastizitätsmodul of 17.6 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 15 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 15 kJ/m² | dry, 50%RH | ISO 179/1eA | |
23 °C | 15 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 15 kJ/m² | dry, 50%RH | ISO 179/1eA | ||
23 °C | 17 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 17 kJ/m² | 50%RH | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | 80 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 80 kJ/m² | dry | ISO 179/1eU | -30°C | |
81 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 81 kJ/m² | 50%RH | ISO 179/1eU | -30°C | ||
95 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 95 kJ/m² | dry | ISO 179/1eU | 23°C | ||
102 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 102 kJ/m² | 50%RH | ISO 179/1eU | 23°C | ||
Zugfestigkeit | 190 MPa Show Supplier Material materials with Zugfestigkeit of 190 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
250 MPa Show Supplier Material materials with Zugfestigkeit of 250 MPa | dry | ISO 527-2/1A | 5mm/min |
Thermisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 1.7e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.7e-05 1/K | ISO 11359-1/-2 | 23°C-55°C |
6.8e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 6.8e-05 1/K | ISO 11359-1/-2 | 23°C-55°C, Transverse | |
Schmelzpunkt | 258 °C Show Supplier Material materials with Schmelzpunkt of 258 °C | ISO 11357-1/-3 | 10°C/min |
Wärmeformbeständigkeitstemperatur | 245 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 245 °C | ISO 75/2Af | 1.80 MPa |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schrumpfung | 0.1 % Show Supplier Material materials with Schrumpfung of 0.1 % | 290/120/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
0.4 % Show Supplier Material materials with Schrumpfung of 0.4 % | 290/120/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Features | Heat Stabilized | |
Fillers | 50% Glass Fiber | |
Processing methods | Injection Molding |