Allgemein
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Dichte | 1.47 g/cm³ Show Supplier Material materials with Dichte of 1.47 g/cm³ | dry | ISO 1183 | |||
Moisture absorption | 23 °C | 1.3 % Show Supplier Material materials with Moisture absorption of 1.3 % | 50%RH | ISO 62 | 2 mm | |
Wasserabsorption | 0.1 % Show Supplier Material materials with Wasserabsorption of 0.1 % | ISO 62 | 2 mm | 24h immersion at 23°C |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Biegefestigkeit | 240 MPa Show Supplier Material materials with Biegefestigkeit of 240 MPa | dry | ISO 178 | 2mm/min | |
Biegemodul | 11 GPa Show Supplier Material materials with Biegemodul of 11 GPa | dry | ISO 178 | 2mm/min | |
Dehnung | 2.2 % Show Supplier Material materials with Dehnung of 2.2 % | 50%RH | ISO 527-2/1A | 5mm/min | |
2.4 % Show Supplier Material materials with Dehnung of 2.4 % | dry | ISO 527-2/1A | 5mm/min | ||
Elastizitätsmodul | 10.9 GPa Show Supplier Material materials with Elastizitätsmodul of 10.9 GPa | dry | ISO 527-2/1A | 1mm/min | |
11 GPa Show Supplier Material materials with Elastizitätsmodul of 11 GPa | 50%RH | ISO 527-2/1A | 1mm/min | ||
Schlagfestigkeit, Charpy gekerbt | 23 °C | 10 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 10 kJ/m² | dry | ISO 179/1eA | |
23 °C | 11 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 11 kJ/m² | 50%RH | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 50 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 50 kJ/m² | dry | ISO 179/1eU | |
23 °C | 55 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 55 kJ/m² | dry | ISO 179/1eU | ||
Zugfestigkeit | 135 MPa Show Supplier Material materials with Zugfestigkeit of 135 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
155 MPa Show Supplier Material materials with Zugfestigkeit of 155 MPa | dry | ISO 527-2/1A | 5mm/min |
Thermisch
Property | Value | Thickness | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | 1 mm, 2 mm | IEC 60695-2-12 | ||||
Glow Wire Ignition Temperature | 800 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 800 °C | 1 mm, 2 mm | IEC 60695-2-13 | ||||
Schmelzpunkt | 305 °C Show Supplier Material materials with Schmelzpunkt of 305 °C | ISO 11357-1/-3 | 10°C/min | ||||
Wärmeformbeständigkeitstemperatur | 280 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 280 °C | ISO 75/2Af | 1.80 MPa | ||||
Entflammbarkeit | Thickness tested (mm): 0.4, Class: V-0, Standard: UL 94 | Thickness tested (mm): 1.5, Class: 5VA, Standard: UL 94 | Thickness tested (mm): 1.5, Class: 5VA, Standard: IEC 60695-11-20 at dry condition (Burning behaviour) |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Durchschlagfestigkeit | 42 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 42 kV/mm | dry | IEC 60243-1 | |
44 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 44 kV/mm | 50%RH | IEC 60243-1 | ||
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | dry | IEC 60112 | Sol.A |
Surface resistivity | 1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schrumpfung | 0.4 % Show Supplier Material materials with Schrumpfung of 0.4 % | 315/120/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
0.9 % Show Supplier Material materials with Schrumpfung of 0.9 % | 315/120/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent, Flame retarding agent | |
Certifications | Yellow Card, RoHS 2011/65/UE | |
Color | Natural | |
Features | Flame Retardant, Heat Stabilized | |
Fillers | 30% Glass Fiber | |
Processing methods | Injection Molding |