Property | Value | Testing Standard |
---|---|---|
Dichte | 1.09 g/cm³ Show Supplier Material materials with Dichte of 1.09 g/cm³ | ISO 1183 |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Biegefestigkeit | 4 MPa Show Supplier Material materials with Biegefestigkeit of 4 MPa | ISO 178 | 2mm/min |
Biegemodul | 0.035 GPa Show Supplier Material materials with Biegemodul of 0.035 GPa | ISO 178 | 2mm/min |
Dehnung | 800 % Show Supplier Material materials with Dehnung of 800 % | ISO 527-2/1A | 50mm/min | nominal |
Elastizitätsmodul | 0.025 GPa Show Supplier Material materials with Elastizitätsmodul of 0.025 GPa | ISO 527-2/1A | 1mm/min |
Härte, Shore D | 22 [-] Show Supplier Material materials with Härte, Shore D of 22 [-] | ISO 7619-1 | 15s |
25 [-] Show Supplier Material materials with Härte, Shore D of 25 [-] | ISO 7619-1 | inst. | |
Modul bei 100 % Dehnung | 0.005 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.005 GPa | ISO 527-2/1A | |
Modul bei 300 % Dehnung | 0.007 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.007 GPa | ISO 527-2/1A | |
Modulus at 10% elongation | 0.002 GPa Show Supplier Material materials with Modulus at 10% elongation of 0.002 GPa | ISO 527-2/1A | |
Schlagfestigkeit, Charpy gekerbt | No Break at 23°C | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | No Break at 23°C | ISO 179/1eU |
Thermisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzpunkt | 175 °C Show Supplier Material materials with Schmelzpunkt of 175 °C | ISO 11357-1/-3 | 10°C/min |
Elektrisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Surface resistivity | 1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | IEC 60093 | 500V |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | IEC 60093 | 500V |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 11.5 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 11.5 g/10min | ISO 1133 | 230°C/2.16Kg |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive | |
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Features | Impact Modified | |
Processing methods | Injection Molding,Profile Extrusion |