Allgemein
Property | Value | Testing Standard | Comment |
---|---|---|---|
Abrasion resistance | 20 mm³ Show Supplier Material materials with Abrasion resistance of 20 mm³ | ISO 4649 | |
Dichte | 1.23 g/cm³ Show Supplier Material materials with Dichte of 1.23 g/cm³ | ISO 1183 | |
Wasserabsorption | 0.2 % Show Supplier Material materials with Wasserabsorption of 0.2 % | ISO 62@1 | immersion at 23°C |
Mechanisch
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Biegefestigkeit | 20 MPa Show Supplier Material materials with Biegefestigkeit of 20 MPa | ISO 178 | 2mm/min | |
Biegemodul | 0.37 GPa Show Supplier Material materials with Biegemodul of 0.37 GPa | ISO 178 | 2mm/min | |
Dehnung | 600 % Show Supplier Material materials with Dehnung of 600 % | ISO 527-2/1A | 50mm/min | nominal | |
Elastizitätsmodul | 0.39 GPa Show Supplier Material materials with Elastizitätsmodul of 0.39 GPa | ISO 527-2/1A | 1mm/min | |
Elongation at yield | 25 % Show Supplier Material materials with Elongation at yield of 25 % | ISO 527-2/1A | 50mm/min | |
Härte, Shore D | 57 [-] Show Supplier Material materials with Härte, Shore D of 57 [-] | ISO 7619-1 | 15s | |
65 [-] Show Supplier Material materials with Härte, Shore D of 65 [-] | ISO 7619-1 | inst. | ||
Modul bei 100 % Dehnung | 0.022 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.022 GPa | ISO 527-2/1A | ||
Modul bei 300 % Dehnung | 0.023 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.023 GPa | ISO 527-2/1A | ||
Modulus at 10% elongation | 0.019 GPa Show Supplier Material materials with Modulus at 10% elongation of 0.019 GPa | ISO 527-2/1A | ||
Reißfestigkeit | 241 kN/m Show Supplier Material materials with Reißfestigkeit of 241 kN/m | ISO 34-1 | ||
Schlagfestigkeit, Charpy gekerbt | 23 °C | 70 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 70 kJ/m² | ISO 179/1eA | |
Streckgrenze | 25 MPa Show Supplier Material materials with Streckgrenze of 25 MPa | ISO 527-2/1A | 50mm/min | |
Zugfestigkeit | 38 MPa Show Supplier Material materials with Zugfestigkeit of 38 MPa | ISO 527-2/1A | 5mm/min |
Thermisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzpunkt | 212 °C Show Supplier Material materials with Schmelzpunkt of 212 °C | ISO 11357-1/-3 | 10°C/min |
Vicat-Erweichungstemperatur | 195 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 195 °C | ISO 306 | 50°C/h 50N |
Wärmeformbeständigkeitstemperatur | 60 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 60 °C | ISO 75/2Af | 1.80 MPa |
110 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 110 °C | ISO 75/2Bf | 0.45 MPa |
Elektrisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Surface resistivity | 1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | IEC 60093 | 500V |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | IEC 60093 | 500V |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 23 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 23 g/10min | ISO 1133 | 230°C/2.16Kg |
Technological properties
Property | ||
---|---|---|
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Features | Impact Modified | |
Processing methods | Injection Molding,Profile Extrusion |