Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 1.17 g/cm³ Show Supplier Material materials with Dichte of 1.17 g/cm³ | ISO 1183 |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Biegefestigkeit | 10 MPa Show Supplier Material materials with Biegefestigkeit of 10 MPa | ISO 178 | 2mm/min |
Biegemodul | 0.135 GPa Show Supplier Material materials with Biegemodul of 0.135 GPa | ISO 178 | 2mm/min |
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | ISO 527-2/1A | 5mm/min |
Elastizitätsmodul | 0.18 GPa Show Supplier Material materials with Elastizitätsmodul of 0.18 GPa | ISO 527-2/1A | 1mm/min |
Härte, Shore D | 48 [-] Show Supplier Material materials with Härte, Shore D of 48 [-] | ISO 7619-1 | 15s |
55 [-] Show Supplier Material materials with Härte, Shore D of 55 [-] | ISO 7619-1 | inst. | |
Modul bei 100 % Dehnung | 0.015 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.015 GPa | ISO 527-2/1A | |
Modul bei 300 % Dehnung | 0.018 GPa Show Supplier Material materials with Modul bei 300 % Dehnung of 0.018 GPa | ISO 527-2/1A | |
Modulus at 10% elongation | 0.009 GPa Show Supplier Material materials with Modulus at 10% elongation of 0.009 GPa | ISO 527-2/1A | |
Modulus at 50% elongation | 0.012 GPa Show Supplier Material materials with Modulus at 50% elongation of 0.012 GPa | ISO 527-2/1A | |
Schlagfestigkeit, Charpy gekerbt | No Break at 23°C and at -30°C | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | No Break at 23°C | ISO 179/1eU |
Thermisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzpunkt | 200 °C Show Supplier Material materials with Schmelzpunkt of 200 °C | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 7 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 7 g/10min | ISO 1133 | 230°C/2.16Kg |
Technological properties
Property | ||
---|---|---|
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Features | Impact Modified, UV Stabilized, Heat Stabilized | |
Processing methods | Profile Extrusion,Other Extrusion |